Key points of construction and application technology of high-strength refractory castables

    High-strength refractory castable refers to a kind of hydraulic high-strength refractory castable made of corundum as aggregate, high-quality high-aluminum cement as binder, and several additives, which is used as a high-temperature and easily worn part of the lining of thermal kilns.

    High-strength refractory castables can be divided into superior and first-class categories according to their performance. The initial setting time of high-strength refractory castables is not less than 30min and not more than 240min.

    High-strength refractory castables are mainly used for high-temperature and easily worn parts of thermal kilns. For example, the kiln mouth in front of the cement pre-decomposition kiln, the three-duct coal injection pipe; the casting or ramming parts of the lining of metallurgical furnaces such as refining spray guns, RH, DH vacuum degassing devices, etc., can also be used as refractory linings for petroleum catalytic devices, etc.

news-800-800

    High-strength refractory castables must be stored in a dry warehouse.

    The following points should be noted during construction:

    (1) The water must be clean and the pH value must be between 6 and 8. The mixing water should be accurately weighed.

    (2) It is recommended to use a forced mixer and all mixing tools must be clean. Mix until the material is uniform.

    (3) The casting surface of the mold used should be coated with a layer of engine oil.

    (4) All embedded metal parts should be coated with a layer of asphalt paint before pouring.

    (5) The high-strength refractory castable should be used within 30 minutes after mixing. It is advisable to pour it to the specified thickness at one time and vibrate it until it is completely dense.

    (6) The curing humidity should not be less than 90%, the curing temperature should be between 15 and 25°C, and the mold should be removed 24 hours after pouring. The total curing time is 3 days.

    (7) The lining or structure made of high-strength refractory castable should be properly heat treated before use. Raise the temperature to 110℃ at a rate of 25℃/h and keep it warm for more than 4h; raise the temperature to 400℃ at a rate of 40℃/h and keep it warm for more than 4h; raise the temperature to the use temperature at a rate of 10-15℃/h; keep the temperature constant at the operating temperature for more than 2d according to the needs and possibilities of different parts.