Silicon mollite brick is a high-performance composite refractory material, specially designed for transition zone and preheat zone of cement rotary kiln, made of silicon carbide, mullite and corundum through high pressure molding and high temperature firing. Its excellent wear resistance, high thermal conductivity and excellent thermal shock resistance make it an ideal material to replace traditional high-alumina bricks and magnesia-chrome bricks.
Installation points
When laying silica mollite bricks, the gaps between the upper and lower bricks should be staggered by ≥100mm to avoid straight seams that will reduce the structural strength. The arc should be uniform when laying in a ring. The mortar filling rate should be ≥95%. Use a rubber hammer to tap the bricks to make them fit tightly to avoid voids or gaps. Leave a 3-5mm expansion joint for every 1m of masonry length, and fill the joint with ceramic fiber or refractory cardboard to avoid embedding of debris. Use special-shaped bricks or cut bricks for splicing at corners and interfaces. The cut surface should be polished and sealed with mud to prevent high-temperature gas penetration.
The transition zone of cement kilns has large temperature fluctuations, so the locking structure between bricks needs to be strengthened during masonry, and silicon carbide fibers need to be embedded in the brick joints to enhance thermal shock resistance. The bottom brick layer of high-temperature load-bearing parts needs to be laid with load-bearing steel plates or refractory concrete cushions to avoid excessive local loads that cause brick cracking.
Usage and maintenance specifications
The first heating is to be raised to 300℃ at a rate of ≤50℃/h and kept at this temperature for 2h; then raised to 600℃ at a rate of ≤80℃/h and kept at this temperature for 4h; then the temperature is raised according to the normal process to avoid sudden cooling and heating. When the kiln is stopped and cooled, it is necessary to naturally cool to below 400℃ before opening the kiln door to avoid direct cold wind blowing on the brick body. Avoid over-temperature use to prevent the decomposition of the mullite phase and the decrease in strength. When in contact with molten materials, the brick surface crust needs to be cleaned regularly to avoid chemical erosion.
Check the brick surface weekly for signs of peeling, cracks or corrosion, paying special attention to whether the expansion joints are blocked or deformed.
Through the above steps, the high temperature performance and durability of silica mollite bricks can be maximized to extend the service life of the equipment. You can consult the professional staff of Haixin Refractory Materials at any time, and we will give the most professional construction plan based on the specific working conditions.