It is a common phenomenon that LS acid resistant putty has surface cracks during construction or use, which may be caused by factors such as material ratio, construction technology, environmental conditions or design defects.
1. Improper material ratio
Excessive curing agent: causes the cement to cure too quickly, increases shrinkage stress, and forms shrinkage cracks.
Excessive filler ratio: reduces the flexibility of the cement, increases brittleness, and is prone to cracking due to external force or temperature difference.
Uneven mixing: local poor curing or uneven strength, forming weak areas.
2. Construction process problems
Too thick a single layer: The thickness of the one-time application exceeds 3mm, and the internal curing heat release is not synchronized with the surface shrinkage, resulting in internal stress cracks.
Unlayered construction: Failure to operate according to the principle of "thin coating and multiple layers", and insufficient curing between layers.
Improper surface treatment: There is oil, floating dust or excessive humidity (>5%) on the surface of the substrate, resulting in insufficient adhesion and cracking.
3. Environmental factors
Sudden temperature change: After construction, the cement will be exposed to high temperature or frozen at low temperature, and the thermal expansion and contraction of the cement will cause cracks.
Excessive humidity: During the curing process, the evaporation of water is blocked, and micropores are generated inside and expand into cracks.
4. Wrong material selection
Failure to select the material according to the working conditions (such as not selecting high-temperature resistant cement in high-temperature environment) leads to insufficient material performance.
Correct construction process of LS acid-resistant cement
1. Base surface treatment:
Remove oil, rust, and loose layers to ensure that the base surface is dry and solid.
The concrete base surface needs to be polished to roughness, and sandblasting is recommended for metal base surfaces.
2. Cement preparation:
Mix resin, curing agent and filler in proportion (strictly follow the product instructions to avoid curing too fast or too slow).
Stir evenly until there is no lumps, and use it now (usually used up within 30 minutes).
3. Application construction:
Use scraping or spatula to apply in layers, with a thickness of 2-3mm per layer and a total thickness based on design requirements (usually 4-8mm).
The interlayer construction should be done after the previous layer is solidified to avoid stratification.
4. Curing and curing:
Curing at room temperature for 24-48 hours, and the curing time needs to be extended in low temperature or high humidity environment.
After complete curing, pickling or putting into use.