Wear-resistant refractory castables are mainly used for high temperature and wear resistance, lining in high temperature areas, and have high requirements for bending strength and compressive strength.
The performance of wear-resistant refractory castables depends on the different proportions of raw materials. Generally, high-strength refractory aggregates and powders and high-strength binders are added. For some key parts, due to harsh conditions, corundum, corundum zirconium corundum, high-alumina bauxite sinter and silicon carbide are added to meet the use requirements.

In many cases, the condition of use is which kind of binding material is added. As long as it is wear-resistant, it will not leave a particle size composition of tight packing. For wear-resistant castables, the wear resistance at room temperature is usually required to be no more than 10cm3.
If the castable is used for circulating fluidized bed boilers in power plants, it is basically made by adding fused corundum and a certain proportion of black silicon carbide. The binder will be pure calcium aluminate cement with silica powder.
If it is used in the lining of an alumina suspension furnace, silicon carbide cannot be added, but sintered white corundum or fused corundum must be added in a certain proportion.
If it is to be added in the steel tank of the heating furnace, sub-white corundum and brown corundum should be added. The powder should be just-melted corundum powder. The micro powder is zircon micro powder.
For wear-resistant castables used in oil refining catalytic cracking units, smelting sintered corundum or plate-shaped corundum must be added in a certain proportion.
If used at a temperature above 1500℃, making prefabricated blocks is also a good choice. If a certain amount of SiC is added to the prefabricated blocks to make the parts of the prefabricated bricks rough, the construction is not only convenient, but also has better high temperature wear resistance.
In short, the use of refractory refractory castables should be based on the actual use temperature and different conditions of furnace erosion. As for the production of prefabricated bricks or castable bricks, it also depends on the situation.