1.Performance advantages of silicon carbide corundum refractory plastic
Silicon carbide corundum refractory plastic is an unshaped refractory material made from high-alumina bauxite clinker, corundum, mullite, and silicon carbide as core aggregates, combined with special binders and additives.
1.1Super wear-resistant and corrosion-resistant:
The carbon SiC content is ≥60%, and the Al₂O₃ content can reach up to 85%. This combination can resist high-temperature airflow, material erosion and chemical corrosion, and its service life is significantly better than that of ordinary wear-resistant plastics.
1.2Convenient and efficient construction:
It can be directly applied and tamped into shape without the need for molds, making it suitable for irregular and worn areas; no oven drying is required after construction, which greatly shortens the construction period.
1.3Excellent high-temperature stability:
The operating temperature can reach 1200℃, and the permanent linear change rate after heating at 850℃ is only -0.6~0%. It has a thermal shock resistance of ≥35 cycles and can withstand rapid temperature fluctuations without cracking. It is suitable for long-term high-temperature working conditions.
1.4High bonding strength:
After molding, it bonds tightly to the substrate. With mesh anchors spaced 120-150mm apart, it can effectively prevent detachment, making it especially suitable for furnace repair and lining construction in complex areas.
2.Application scenarios of silicon carbide corundum refractory plastic
Silicon carbide corundum refractory plastics are widely used in high-temperature critical components across multiple industries:
2.1Power industry: Highly abrasive areas of circulating fluidized bed boilers, such as the combustion zone, cyclone separator, return riser, heat radiation material zone, and tail flue, as well as boiler door filling and cold slag machine lining repair.
2.2 Metallurgy and Iron: High-temperature wear-resistant linings for heating furnaces and calcining furnaces, and parts subject to material erosion such as blast furnace hot blast stove pipes and cyclone dust collector inner walls.
2.3 Ceramic building materials: preheating zone and firing zone lining of ceramic kilns, transition zone of cement rotary kilns, decomposition furnace and other high-temperature dust scouring areas.
2.4 General Industrial Applications: Repairing irregular wear parts of various high-temperature kilns and forming irregularly shaped linings, especially suitable for emergency repair scenarios, requiring no maintenance or waiting.
3. Construction Guidelines
3.1Pre-construction preparation
3.1.1Substrate preparation: The construction surface must be cleaned of dirt and dust, coated with asphalt paint and allowed to dry completely; anchor nails should be welded according to the design, with a spacing of 120-150mm.
3.1.2Equipment preparation: Equip with a forced mixer, tamping machine, measuring bucket, weighing scale, trimming knife, wire brush, etc. The mixer must be cleaned in advance to remove any debris.
3.2Mixing and molding
3.2.1Mixing ratio control: The matrix material, binder, and accelerator are packaged separately. The mixing ratio is adjusted according to the season. The construction site temperature should be 5-25℃. After the dry-mixed matrix material is mixed for 2 minutes, the binder is added and stirred for 5 minutes. Finally, the accelerator is added and stirred for 1-2 minutes.
3.2.2Construction time: It must be used within 40 minutes after mixing to avoid the material solidifying and becoming ineffective; use tamping or spreading process, tamping must be dense and flat, the thickness of a single construction should be as required by the design, and the maximum should not exceed 60mm. When construction is intermittent, the tamped surface should be covered with plastic sheeting to prevent it from drying out.
3.2.3Post-processing: After molding, promptly trim the surface and roughen any unremoved parts; open 4-6mm ventilation holes on the heated surface and cut expansion joints 5mm wide and 50-80mm deep according to the design.
3.3Maintenance and Crack Treatment
3.3.1Natural curing: After construction, cure in a dry environment at 15-35℃ for 5-7 days, avoiding vibration and water contact; if the furnace cannot be dried in time, cover it with plastic sheeting, and the formation of small water droplets on the inner lining surface is a normal phenomenon.
3.3.2Crack repair: When the width is 1-3mm, spray water to moisten and then gently tap to close; when the width is 3-5mm (high temperature area) or 3-12mm (normal area), fill with mud or plastic; when the width is more than 5mm (high temperature area) or 12mm (normal area), dig a wedge-shaped opening that is larger inside and smaller outside, moisten and then fill with plastic.
4.Store
4.1Environmental requirements: Store in a cool, damp place in summer and take precautions against freezing in winter; do not store with acidic or alkaline substances to prevent deterioration.
4.2Shelf life management: Materials that have exceeded their shelf life must be retested for plasticity index (should be between 15-40%), and those that fail to meet the standard shall not be used; materials stored for 1 year must be re-dried before use.
Silicon carbide corundum refractory plastic, with its advantages of wear and corrosion resistance, convenient construction, and high-temperature stability, has achieved practical value in cost reduction and efficiency improvement in high-temperature industrial fields: construction cycle is shortened by more than 30%, maintenance costs are reduced by 50%, and the service life of the lining is extended by 2-3 times compared with ordinary materials. By strictly following the selection standards, standardized construction, and standardized storage, its performance advantages can be maximized. It is suitable for the construction and maintenance of kilns in industries such as power, metallurgy, and ceramics, and is especially suitable for construction in complex parts and emergency repair scenarios.