Related Knowledge Of Fused-cast Zirconium Corundum Bricks

Mar 25, 2025

Leave a message

    Cast zirconium corundum bricks are commonly known as tin bricks. They are the most important refractory materials to ensure the normal operation of glass melting furnaces. At present, the improvement of melting rate, extension of kiln life and reduction of fuel consumption in glass melting furnaces at home and abroad are mainly achieved by using this refractory material.

    Fused-cast zirconium corundum bricks can also be called corundum-badgezircon products. The main chemical composition is 50%~70% Al2O3, 20%~40% ZrO2, and the rest is SiO2. The main mineral components are baddeleyite (ZrO2), corundum (α-Al2O3) and glass phase.

Baddeleyite crystals form the backbone of the brick. ZrO2 has a high melting point (2715°C), good chemical stability, and strong resistance to corrosion in acidic and alkaline media, especially in glass liquid.

    The following issues should be noted during use:

    (1)Irregular changes in thermal expansion. The expansion curve of the fused-cast zirconium corundum brick has an abnormal section near 1000℃, and the ZrO2 crystal inside it undergoes a reversible crystal transformation, with a large volume change. Therefore, products containing ZrO2 should not be used in areas around 1000℃ where the temperature often fluctuates sharply. When baking the furnace and kiln, the temperature change should not be too large at 900-1150℃, generally not more than 15℃/h, and a steady temperature rise is required. Some parts should be protected from cold wind and need to be protected with other bricks to prevent cracking.

    (2)Shrinkage holes. Shrinkage holes often appear at the casting mouth during casting. The bricks here have many pores and poor density. Therefore, when building the glass melting pool wall, the shrinkage holes are all facing the inside of the kiln. If the casting mouth faces outward, when the bricks are eroded to a very thin layer, it will cause glass liquid leakage accidents. When used in the flame space above the pool kiln, the service life is very long and there will be no glass liquid leakage problem. Therefore, the casting mouth is used outward to extend the service life.

    (3)Eutectic. When cast zirconium corundum bricks are placed in contact with clay bricks, eutectic phenomenon will occur at a high temperature of 1300℃. Therefore, when selecting refractory materials, it is necessary to avoid placing two refractory materials with serious eutectic phenomenon in contact with each other. For example, silica bricks are most susceptible to erosion by cast zirconium corundum bricks under fused zirconium corundum bricks.

    The fused-cast zirconium corundum products for glass kilns are divided into three grades according to their zirconium oxide content: AZS-33 with a nominal zirconium oxide content of 33%; AZS-36 with a nominal zirconium oxide content of 36%; and AZS-41 with a nominal zirconium oxide content of 41%.

    Haixin Refractory can customize fused cast zirconium corundum special-shaped products according to user needs. The size tolerance and appearance index of special-shaped products shall be agreed upon by both parties. The size tolerance and appearance index of special-shaped products shall be agreed upon by both parties. The crack index of dense and shrinkage-free products shall be agreed upon by both parties. No molding sand or other sintered materials shall be attached to the surface of the product.